prEN ISO 11357-5
Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion (ISO/DIS 11357-5:2024)
Draft Public enquiryProject stage codes
1. Nauja darbo tema
2. Projektas
3. Viešoji apklausa
From 2024-04-18
till 2024-06-27
4. Closure of enquiry
5. Projekto priėmimas
Organisation
CEN Europos standartizacijos komitetasTechnical Committee
TK 68 PlasticsForeignTC'S
CEN/TC 249Number of comments
0Comment start date
2024-04-18Scope
ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC). The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.Relations