prEN ISO 11357-6
Plastics - Differential scanning calorimetry (DSC) - Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) (ISO/DIS 11357-6:2024)
Draft Archived
Comment end date
2024-04-26
Project stage codes
1. Nauja darbo tema
2. Projektas
3. Viešoji apklausa
From 2024-02-15
till 2024-04-26
4. Closure of enquiry
5. Projekto priėmimas
Organisation
CEN Europos standartizacijos komitetasICS
83.080.01 - Plastics in generalTechnical Committee
TK 68 PlasticsForeignTC'S
CEN/TC 249Number of comments
0Comment start date
2024-02-15Scope
ISO 11357-6:2018 specifies methods for the determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) of polymeric materials by means of differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized or compounded form, either as raw materials or finished products. It can be applicable to other plastics.Relations